Into | Iinkcukacha |
Umbala | Okusekuhleni |
Izinga lomxube | 2:1:0.3 |
Ukutshiza ukutyabeka | 2-3 umaleko,40-60um |
Isithuba sexesha(20°) | 5-10 imizuzu |
Ixesha lokumisa | Umphezulu womile imizuzu engama-45, ukhazimliswe iiyure ezili-15. |
Ixesha elikhoyo (20°) | 2-4 iiyure |
Isixhobo sokutshiza kunye nokugalela | Umpu wokutshiza we-Geocentric(ibhotile ephezulu) 1.2-1.5mm;3-5kg/cm² |
Umpu wokufunxa (ibhotile esezantsi) 1.4-1.7mm;3-5kg/cm² | |
Ithiyori ubuninzi bepeyinti | I-2-3 imigangatho malunga ne-3-5㎡/L |
Ubomi bokugcina | Gcina ngaphezu kweminyaka emibini kwisikhongozeli sokuqala. |
. Yenza ukulungiswa ngokukhawuleza okusebenzayo
.Yehlisa iziphene zepeyinti
. Ukuguquguquka kwezixhobo zokumisa
.Ukusetyenziswa kwezinto ngokufanelekileyo
I-1, isebenza kwipeyinti ephantsi ephantsi kwaye ecociweyo ephakathi, ipeyinti yokuqala okanye umgangatho wepeyinti we-2K.Kwaye izinto ezithambileyo ezisekelwe kwi-insulating layer.
I-2, ingasetyenziselwa ukutshiza inxalenye yeemoto ezintsha okanye ukulungiswa kweemoto ezindala.
Ifilim yepeyinti endala eyenziwe lukhuni yaze yapolishwa, umphezulu kufuneka wome kwaye ungabi nabumdaka obufana negrisi.
1.Tyaza kangangoko kunokwenzeka, iimeko ezikhethekileyo zinokuba yi-brush coating;
2. Ipeyinti kufuneka ixutywe ngokulinganayo ngexesha lokwakhiwa, kwaye ipeyinti kufuneka ihlanjululwe nge-solvent ekhethekileyo kwi-viscosity efunekayo ekwakheni.
3. Ngexesha lokwakha, umphezulu kufuneka wome kwaye ucocwe ngothuli.
4.Spray 2-3 layers, unokupolisha emva kweeyure eziyi-15.
1.Base lobushushu nahayi ngaphantsi kwe-5°C, ukufuma okunxulumene nama-85% (iqondo lobushushu kunye nokufuma okunxulumeneyo kufuneka kulinganiswe kufutshane nemathiriyeli esisiseko), inkungu, imvula, ikhephu, umoya nemvula aluvumelekanga ngokungqongqo ulwakhiwo.
2.Ngaphambi kokupeyinta ipeyinti,coca indawo egqunyiweyoukuphepha ukungcola kunye neoli.
3.Imveliso inokutshizwa, kucetyiswa ukutshiza ngezixhobo ezikhethekileyo.Ububanzi bombhobho yi-1.2-1.5mm, ubukhulu befilimu yi-40-60um.